965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

BLOOM(suzhou) Materials Co.,Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

Brand Name : BLM-DX-1

Place of Origin : Jiangsu, China (Mainland)

MOQ : 100kgs

Price : FobShanghai usd 5.9-6.4/kg

Payment Terms : Western Union, L/C, T/T

Supply Ability : 300 Ton/Tons per Month

Delivery Time : 25-30 days subject to the clients' requirement and quantity

Packaging Details : packed and labeled according to the regulations and customer's requests.Great care is taken to avoid any damage which might otherwise be caused during storage or transportation.

Standard : AISI, ASTM, BS, DIN, GB, JIS, Other,JIS,AISI,ASTM,GB,DIN,EN

Grade : Inconel 718

Thickness : 8mm-100mm

Type : Tube / pipe

Dimensions : 10-900MM

Length : 2m,3m or as required

Special Use : Cold Heading Steel

Delivery : 25-30 days subject to the clients' requirements and quantity

Price Term : Ex-Work,FOB,CNF,CFR,CIF,FCA,DDP,DDU

Surface Treatment : bright&smooth

Application : Structural Steel Bar

Contact Now

Inconel 718

Inconel 718 Chemical composition

Alloy % Ni Cr Fe Mo Nb Co C Mn Si S Cu Al Ti
718 Min. 50 17 balance 2.8 4.75 0.2 0.7
Max. 55 21 3.3 5.5 1 0.08 0.35 0.35 0.01 0.3 0.8 1.15

Inconel 718 Physical properties

Density 8.2 g/cm³
Melting point 1260-1340 ℃

Inconel 718 Alloy minimum mechanical properties in the roomtemperature

Alloy Tensile strength Rm N/mm² Yield strength R P0. 2N/mm² Elongation A 5 %

Brinell hardness

HB

Solution treatment 965 550 30 ≤363

718 Characteristic as below:

1.workability

2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.

3.High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.

5.Good welding performance.

Inconel 718 Metallurgical structure

718alloy is Austenitic structure, precipitation hardening generate "γ" made it excellent mechanical performance. G rain boundary generate "δ" made it the best plasticity in the heat treatment.

Inconel 718 Corrosion resistance

718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.

Inconel 718 Application field:

1 . The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties

2 . made it use in a wide range of high requirement environments :Steam turbine ; Liquid-fuel rocket ; Cryogenic engineering

3.Acid environment

4.Nuclear engineering

965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance


Product Tags:

inconel 625 material

      

inconel 718 material

      
Wholesale 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from china suppliers

965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: BLOOM(suzhou) Materials Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)